CNS 631 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of CNS 631

Location » Home » Grades > Stainless Steels > CNS 631

CNS CNS 631

Profile

This page is mainly introduced the CNS 631 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of CNS 631,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel bars

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.09
Si   1.00
Mn   1.00
P   0.040
S   0.030
Ni 6.50  7.75
Cr 16.00  18.00
Cu  
Al 0.75  1.50

Mechanical Properties

Tensile strength 389~947 σb/MPa
Yield Strength 087 σ 0.2 ≥/MPa
Elongation 66 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 512~697 -
HRC 30 -

Physical Properties

Thermal expansion 36-70 e-6/K
Thermal conductivity 52-56 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 1981-2757 째C
Density 1133-9829 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
CNS 631 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk