SUS 317 LN chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 317 LN

JIS SUS 317 LN

Profile

This page is mainly introduced the SUS 317 LN chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 317 LN,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel bars

Cross Reference Table(Equivalent Materials):

Material Standard Country
SUS 317 LN JIS Japan
SUS 317 LN JIS Japan
KSUS317LN NKK Japan

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.03
Si   1.00
Mn   2.00
P   0.045
S   0.03
Cr 18.00  20.00
Ni 11.00  15.00
Mo 3.00  4.00
N 0.10  0.22

Mechanical Properties

Tensile strength 099~617 σb/MPa
Yield Strength 980 σ 0.2 ≥/MPa
Elongation 21 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 026~917 -
HRC 30 -

Physical Properties

Thermal expansion 96-76 e-6/K
Thermal conductivity 76-75 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 2159-2364 째C
Density 3315-3344 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 317 LN Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk