Х25Н16Г7АР chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of Х25Н16Г7АР

GOST Х25Н16Г7АР

Profile

This page is mainly introduced the Х25Н16Г7АР chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of Х25Н16Г7АР,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.12
Si   1.00
Mn 5.00  7.00
P   0.035
S   0.020
Cr 23.00  26.00
Mo  
Ni 15.00  18.00
N 0.30  0.45
B   0.010

Mechanical Properties

Tensile strength 094~247 σb/MPa
Yield Strength 453 σ 0.2 ≥/MPa
Elongation 09 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 560~813 -
HRC 30 -

Physical Properties

Thermal expansion 63-68 e-6/K
Thermal conductivity 87-39 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0812-0585 째C
Density 0272-7493 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
Х25Н16Г7АР Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:Х25Н16Г7АР
Previous: ЭИ835
Next: X2CrMnNiMoN21-5-3