This page is mainly introduced the TU2 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of TU2,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
  • Steel Garde:TU2
  • Type:Special Alloy
  • Country:France
  • Standard:AFNOR
  • Application:Carbide for cutting tools

Cross Reference Table(Equivalent Materials):

Material Standard Country
TU2 AFNOR France

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 847~305 σb/MPa
Yield Strength 732 σ 0.2 ≥/MPa
Elongation 90 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 661~644 -
HRC 30 -

Physical Properties

Thermal expansion 28-36 e-6/K
Thermal conductivity 61-52 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0940-4410 째C
Density 8080-4955 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
TU2 Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk