This page is mainly introduced the XГC chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of XГC,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
  • Steel Garde:XГC
  • Type:Special Alloy
  • Country:Russia
  • Standard:ГОСТ
  • Application:XГC

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 442~363 σb/MPa
Yield Strength 668 σ 0.2 ≥/MPa
Elongation 45 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 481~399 -
HRC 30 -

Physical Properties

Thermal expansion 13-35 e-6/K
Thermal conductivity 08-85 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0283-7034 째C
Density 3553-4606 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

√

√

√

√

√

Size Availability

Steel Grade Specification Processing range(mm)
XГC Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk