C125W chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of C125W

Location » Home » Grades > Special Alloy > C125W

DIN C125W

Profile

This page is mainly introduced the C125W chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of C125W,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
C125W
  • Steel Garde:C125W
  • Type:Special Alloy
  • Country:Germany
  • Standard:DIN
  • Application:Carbon tool steel

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 631~444 σb/MPa
Yield Strength 405 σ 0.2 ≥/MPa
Elongation 75 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 817~689 -
HRC 30 -

Physical Properties

Thermal expansion 67-42 e-6/K
Thermal conductivity 59-39 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 6393-6811 째C
Density 5100-1238 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

√

√

√

√

√

Size Availability

Steel Grade Specification Processing range(mm)
C125W Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk