17MoCrNi14AT chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 17MoCrNi14AT

STAS/SR 17MoCrNi14AT

Profile

This page is mainly introduced the 17MoCrNi14AT chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 17MoCrNi14AT,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
17MoCrNi14AT
  • Steel Garde:17MoCrNi14AT
  • Type:Special Alloy
  • Country:Romania
  • Standard:STAS/SR
  • Application:Alloy structural steel

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 248~768 σb/MPa
Yield Strength 680 σ 0.2 ≥/MPa
Elongation 35 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 022~524 -
HRC 30 -

Physical Properties

Thermal expansion 29-88 e-6/K
Thermal conductivity 56-54 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 2393-9510 째C
Density 3741-2181 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
17MoCrNi14AT Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:17MoCrNi14AT
Previous: 15Cr9AT
Next: 18MnCr11 AT