37CrNi3 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 37CrNi3

Location » Home » Grades > Special Alloy > 37CrNi3

GBT 37CrNi3

Profile

This page is mainly introduced the 37CrNi3 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 37CrNi3,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
37CrNi3
  • Steel Garde:37CrNi3
  • Type:Special Alloy
  • Country:China
  • Standard:GBT
  • Application:China structural steel and alloy steel

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 514~704 σb/MPa
Yield Strength 374 σ 0.2 ≥/MPa
Elongation 90 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 658~815 -
HRC 30 -

Physical Properties

Thermal expansion 87-31 e-6/K
Thermal conductivity 84-72 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 3631-1223 째C
Density 0884-6517 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
37CrNi3 Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:37CrNi3
Previous: 30CrNi3
Next: 12CrNi4