1.7336 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 1.7336

Location » Home » Grades > Structural Steel > 1.7336

EN 1.7336

Profile

This page is mainly introduced the 1.7336 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 1.7336,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
EN 1.7336 steel is an alloy steel formulated for primary forming into wrought products. 1.7336 is the EN numeric designation for this material. 13CrMoSi5-5 is the EN chemical designation. It has a moderately low thermal conductivity among EN wrought alloy steels. In addition, it has a moderately high base cost and a fairly low tensile strength.
  • Steel Garde:1.7336
  • Type:Structural Steel
  • Country:European
  • Standard:EN
  • Standard Number:
    ITEM Standard Number Descriptions
    1 EN 10028-2-2009 Flat products made of steels for pressure purposes. Non-alloy and alloy steels with specified elevated temperature properties
  • Application:Flat products made of steels for pressure purposes. Non-alloy and alloy steels with specified elevated temperature properties

Relevant products:

  • 1.7336(13CrMoSi5-5) Plate Sheet

    1.7336(13CrMoSi5-5) Plate Sheet

  • Cross Reference Table(Equivalent Materials):

    Material Standard Country
    13CrMoSi5-5 EN European

    Chemical composition(mass fraction)(wt.%)

    Elements Min.(≥) Max.(≤) Similar Remarks
    C   0.17
    Si 0.50  0.80
    Mn 0.40  0.65
    P   0.015
    S   0.005
    Cr 1.00  1.50
    Ni   0.30
    Mo 0.45  0.65
    N   0.012
    Cu   0.013

    Mechanical Properties

    Tensile strength 245~922 σb/MPa
    Yield Strength 543 σ 0.2 ≥/MPa
    Elongation 13 δ5≥(%)
    ψ - ψ≥(%)
    Akv - Akv≥/J
    HBS 744~639 -
    HRC 30 -

    Physical Properties

    Thermal expansion 23-80 e-6/K
    Thermal conductivity 51-53 W/m.K
    Specific heat 450-460 J/kg.K
    Melting temperature 9723-8352 째C
    Density 9908-5279 kg/m3
    Resistivity 0.50-0.60 Ohm.mm2/m
         

    Heat Treatment Regime

    Annealing

    Quenching

    Tempering

    Normalizing

    Q & T

    Size Availability

    Steel Grade Specification Processing range(mm)
    1.7336 Structural Steel Round Bar and Hollow Bar Φ1 to Φ2000
    Square and Flat Steel Φ10 to Φ100
    Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
    Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
    Coil and Strip Steel THK:0.1mm Width:1500mm
    Forged Ring/Cylindrical/Disk