This page is mainly introduced the 125Cr1 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 125Cr1,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Low alloyed Cr steel

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.20  1.30
Si 0.15  0.30
Mn 0.25  0.40
P   0.030
S   0.030
Cr 0.30  0.40
Mo  
V  

Mechanical Properties

Tensile strength 673~818 σb/MPa
Yield Strength 907 σ 0.2 ≥/MPa
Elongation 96 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 678~062 -
HRC 30 -

Physical Properties

Thermal expansion 72-02 e-6/K
Thermal conductivity 62-75 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 1659-3775 째C
Density 0629-7208 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
125Cr1 Tool Die Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm