2VPermcndur chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 2VPermcndur

Whole 2VPermcndur

Profile

This page is mainly introduced the 2VPermcndur chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 2VPermcndur,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
High temperature alloys and other special alloys

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
Co 49 
V 2.00 

Mechanical Properties

Tensile strength 370~446 σb/MPa
Yield Strength 130 σ 0.2 ≥/MPa
Elongation 24 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 522~103 -
HRC 30 -

Physical Properties

Thermal expansion 62-23 e-6/K
Thermal conductivity 12-05 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 1600-2544 째C
Density 2338-6299 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
2VPermcndur Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk