HS 556 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of HS 556

Location » Home » Grades > Stainless Steels > HS 556

UNS HS 556

Profile

This page is mainly introduced the HS 556 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of HS 556,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta - 0.30Al - 0.05Zr - 0.05La - 0.20N Solution Heat Treated
  • Steel Garde:HS 556
  • Type:Stainless Steels
  • Country:USA
  • Standard:UNS
  • Standard Number:
    ITEM Standard Number Descriptions
    1 SAE AMS 5874C (2007) Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta - 0.30Al - 0.05Zr - 0.05La - 0.20N Solution Heat Treated
  • Metallographic Structure:Precipitation-Hardening
  • Application:Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta - 0.30Al - 0.05Zr - 0.05La - 0.20N Solution Heat Treated

Cross Reference Table(Equivalent Materials):

Material Standard Country
HS-21 UNS USA
HS-31 UNS USA
HS 556 ASTM USA
HS 556 ASTM USA
HS 556 ASTM USA
HS 556 UNS USA
HS 556 UNS USA

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05  0.15
Si 0.20  0.80
Mn 0.50  2.00
Ni 19.00  22.50
Cr 21.00  23.00
Al 0.10  0.50
Cu  
Ti  
Fe   remaining
Mo 2.50  4.00
Co 16.00  21.00
W 2.00  3.50

Mechanical Properties

Tensile strength 669~975 σb/MPa
Yield Strength 575 σ 0.2 ≥/MPa
Elongation 17 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 879~935 -
HRC 30 -

Physical Properties

Thermal expansion 81-76 e-6/K
Thermal conductivity 05-21 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 8707-2058 째C
Density 3830-9396 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
HS 556 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download