Udimet 500 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of Udimet 500

SAE Udimet 500

Profile

This page is mainly introduced the Udimet 500 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of Udimet 500,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Alloy Castings, Investment, Corrosion and Heat Resistant 53Ni - 18Cr - 18Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution and Precipitation Heat Treated
  • Steel Garde:Udimet 500
  • Type:Stainless Steels
  • Country:USA
  • Standard:SAE
  • Standard Number:
    ITEM Standard Number Descriptions
    1 SAE AMS 5384E (1986) Alloy Castings, Investment, Corrosion and Heat Resistant 53Ni - 18Cr - 18Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution and Precipitation Heat Treated
  • Metallographic Structure:Precipitation-Hardening
  • Application:Alloy Castings, Investment, Corrosion and Heat Resistant 53Ni - 18Cr - 18Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Vacuum-Melted, Vacuum-Cast, Solution and Precipitation Heat Treated

Cross Reference Table(Equivalent Materials):

Material Standard Country
Udimet 500 AMS USA
Udimet 500 AMS USA
Udimet 500 SAE USA
Udimet 500 SAE USA

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05  0.10
Si   0.10
Mn   0.10
Cr   19.00
Ni   remaining
Mo   4.00
Co   19.00
W  
Al   3.00
Cu  
Ti   3.00
Fe  
Zr   0.06
B   0.005

Mechanical Properties

Tensile strength 737~885 σb/MPa
Yield Strength 619 σ 0.2 ≥/MPa
Elongation 16 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 972~765 -
HRC 30 -

Physical Properties

Thermal expansion 49-15 e-6/K
Thermal conductivity 84-46 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 1330-3010 째C
Density 8101-4364 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
Udimet 500 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download