SUS 403 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 403

Location » Home » Grades > Stainless Steels > SUS 403

JIS SUS 403

Profile

This page is mainly introduced the SUS 403 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 403,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel wires

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.15
Si   0.50
Mn   1.00
P   0.04
S   0.03
Cr 11.50  13.00
Ni   0.60
Mo  
N  

Mechanical Properties

Tensile strength 296~855 σb/MPa
Yield Strength 299 σ 0.2 ≥/MPa
Elongation 55 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 734~096 -
HRC 30 -

Physical Properties

Thermal expansion 48-89 e-6/K
Thermal conductivity 70-91 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0819-2748 째C
Density 5684-7156 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 403 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download