SUS 410 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 410

Location » Home » Grades > Stainless Steels > SUS 410

JIS SUS 410

Profile

This page is mainly introduced the SUS 410 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 410,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Heat-resisting steel bars and wire rods

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.15
Si   1.00
Mn   1.00
P   0.04
S   0.03
Cr 11.50  13.50
Ni   0.60
Mo  
N  

Mechanical Properties

Tensile strength 112~892 σb/MPa
Yield Strength 285 σ 0.2 ≥/MPa
Elongation 82 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 689~725 -
HRC 30 -

Physical Properties

Thermal expansion 36-58 e-6/K
Thermal conductivity 86-69 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 4208-9864 째C
Density 7576-3976 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 410 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download