SUS 321 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 321

Location » Home » Grades > Stainless Steels > SUS 321

JIS SUS 321

Profile

This page is mainly introduced the SUS 321 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 321,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Heat-resisting steel bars and wire rods

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.08
Si   1.00
Mn   2.00
P   0.045
S   0.03
Cr 17.00  19.00
Ni 9.00  13.00
Mo  
N  
Ti 5×C% 

Mechanical Properties

Tensile strength 235~272 σb/MPa
Yield Strength 941 σ 0.2 ≥/MPa
Elongation 61 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 343~989 -
HRC 30 -

Physical Properties

Thermal expansion 80-53 e-6/K
Thermal conductivity 13-55 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 1530-2844 째C
Density 6799-8696 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 321 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download