HR55 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of HR55

Location » Home » Grades > Stainless Steels > HR55

B.S. HR55

Profile

This page is mainly introduced the HR55 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of HR55,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)
  • Steel Garde:HR55
  • Type:Stainless Steels
  • Country:UK
  • Standard:B.S.
  • Standard Number:
    ITEM Standard Number Descriptions
    1 BS 2HR 55 (2010) Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)
    2 BS HR 55 Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)
  • Application:Specification for nickel-iron-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (Ni/Co 43.5, Cr 16.5, Mo 3.3, Al 1.2, Ti 1.2, Fe remainder)

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04  0.08
Si   0.50
Mn   0.20
P  
S   0.015
Cr 15.50  17.50
Ni 42.00  45.00
Mo 2.80  3.80
Co   2.00
Ti 1.10  1.30
Fe   remaining
Al 1.10  1.30
Cu   0.50
B   0.005
Pb   0.0015
Bi   0.0001
Ag   0.0005
Zr 0.01  0.04

Mechanical Properties

Tensile strength 589~390 σb/MPa
Yield Strength 389 σ 0.2 ≥/MPa
Elongation 65 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 270~649 -
HRC 30 -

Physical Properties

Thermal expansion 02-82 e-6/K
Thermal conductivity 42-43 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 7640-2972 째C
Density 7271-5900 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
HR55 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:HR55
Previous: HR53
Next: HR203