00Cr17Ni13Mo2N chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 00Cr17Ni13Mo2N

GB 00Cr17Ni13Mo2N

Profile

This page is mainly introduced the 00Cr17Ni13Mo2N chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 00Cr17Ni13Mo2N,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
00Cr17Ni13Mo2N

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.030
Si   1.00
Mn   2.00
P   0.035
S   0.030
Ni 10.50  14.50
Cr 16.00  18.50
Mo 2.00  3.00
N 0.12  0.22

Mechanical Properties

Tensile strength 505~660 σb/MPa
Yield Strength 545 σ 0.2 ≥/MPa
Elongation 51 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 808~493 -
HRC 30 -

Physical Properties

Thermal expansion 58-03 e-6/K
Thermal conductivity 30-21 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 5521-9993 째C
Density 2518-1293 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
00Cr17Ni13Mo2N Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm