GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2 4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Location » Home » Products > Superalloy > Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Quick Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2 4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Delivery

  • Delivery status: Forged 、Solutioned 、
  • Surface: Polished 、
  • Standard: ASTM
  • Shape: Round, Flat, Square, Hexagon, Plate, Sheet, Other

Inventory Status

Order

Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1 Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded

Product Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or  to ASTM B637 or WK 2.4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Grade

2.4952

Nimonic 80A

C

0.04~0.10

≤0.10

Si

≤1.00

≤1.00

Mn

≤1.00

≤1.00

P

≤0.020

—

S

≤0.015

≤0.015

Ni

≥65.00

Balance

Cr

18.00~21.00

18.00~21.00

Ti

1.80~2.70

1.80~2.70

Al

1.00~1.80

1.00~1.80

Co

≤1.00

≤2.00

Fe

≤1.50

≤3.00

Cu

≤0.20

≤0.20

B

≤0.008

≤0.008

Zr

—

≤0.15

Pb

—

≤0.0025