17 254 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 17 254

Location » Home » Grades > Special Alloy > 17 254

CSN 17 254

Profile

This page is mainly introduced the 17 254 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 17 254,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
17 254
  • Steel Garde:17 254
  • Type:Special Alloy
  • Country:Czech Republic
  • Standard:CSN
  • Application:The Czech republic Stainless steel

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 600~441 σb/MPa
Yield Strength 679 σ 0.2 ≥/MPa
Elongation 16 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 414~876 -
HRC 30 -

Physical Properties

Thermal expansion 51-94 e-6/K
Thermal conductivity 99-66 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 4920-1432 째C
Density 5174-4364 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
17 254 Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk