2618 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 2618

Location » Home » Grades > Stainless Steels > 2618

ASTM 2618

Profile

This page is mainly introduced the 2618 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 2618,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Aluminum Alloy, Die and Hand Forgings, Rolled Rings, and Forging Stock 2.3Cu - 1.6Mg - 1.1Fe - 1.0Ni - 0.18Si - 0.07Ti (2618-T61) Solution and Precipitation Heat Treated
  • Steel Garde:2618
  • Type:Stainless Steels
  • Country:USA
  • Standard:ASTM
  • Standard Number:
    ITEM Standard Number Descriptions
    1 SAE AMS 4132F (2008) Aluminum Alloy, Die and Hand Forgings, Rolled Rings, and Forging Stock 2.3Cu - 1.6Mg - 1.1Fe - 1.0Ni - 0.18Si - 0.07Ti (2618-T61) Solution and Precipitation Heat Treated
    2 SAE AMS QQ A 367D (2012) Aluminum alloy forgings
    3 SAE AMS A 22771C (2012) Aluminum Alloy Forgings, Heat Treated
  • Metallographic Structure:Precipitation-Hardening
  • Application:Aluminum Alloy, Die and Hand Forgings, Rolled Rings, and Forging Stock 2.3Cu - 1.6Mg - 1.1Fe - 1.0Ni - 0.18Si - 0.07Ti (2618-T61) Solution and Precipitation Heat Treated

Relevant products:

  • 1.4980 Round Bar

    1.4980 Round Bar

  • Chemical composition(mass fraction)(wt.%)

    Elements Min.(≥) Max.(≤) Similar Remarks
    C   0.06
    Si   0.75
    Mn   0.75
    P  
    S  
    Ni   0.50
    Cr 25.00  27.00
    Al  
    Cu   0.20
    Ti  
    Fe  
    N   0.04
    Mo 0.75  1.50

    Mechanical Properties

    Tensile strength 085~057 σb/MPa
    Yield Strength 053 σ 0.2 ≥/MPa
    Elongation 11 δ5≥(%)
    ψ - ψ≥(%)
    Akv - Akv≥/J
    HBS 189~848 -
    HRC 30 -

    Physical Properties

    Thermal expansion 13-21 e-6/K
    Thermal conductivity 50-26 W/m.K
    Specific heat 450-460 J/kg.K
    Melting temperature 8591-8558 째C
    Density 4929-3336 kg/m3
    Resistivity 0.50-0.60 Ohm.mm2/m
         

    Heat Treatment Regime

    Annealing

    Quenching

    Tempering

    Normalizing

    Q & T

    Size Availability

    Steel Grade Specification Processing range(mm)
    2618 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
    Square and Flat Steel Φ10 to Φ100
    Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
    Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
    Coil and Strip Steel THK:0.1mm Width:1500mm
    Forged Ring/Cylindrical/Disk

    Technical specification/standard for download