SUS 430 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 430

Location » Home » Grades > Stainless Steels > SUS 430

JIS SUS 430

Profile

This page is mainly introduced the SUS 430 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 430,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel wire rods

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.12
Si   0.75
Mn   1.00
P   0.04
S   0.03
Cr 16.00  18.00
Ni   0.60
Mo  
N  

Mechanical Properties

Tensile strength 283~570 σb/MPa
Yield Strength 559 σ 0.2 ≥/MPa
Elongation 10 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 067~588 -
HRC 30 -

Physical Properties

Thermal expansion 65-32 e-6/K
Thermal conductivity 61-92 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 8874-2628 째C
Density 8137-0102 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 430 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download