This page is mainly introduced the SUS 430 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 430,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Cold finished stainless steel bars

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.12
Si   0.75
Mn   1.00
P   0.04
S   0.03
Cr 16.00  18.00
Ni   0.60
Mo  
N  

Mechanical Properties

Tensile strength 254~934 σb/MPa
Yield Strength 722 σ 0.2 ≥/MPa
Elongation 76 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 849~116 -
HRC 30 -

Physical Properties

Thermal expansion 00-52 e-6/K
Thermal conductivity 99-36 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 2325-1525 째C
Density 5013-8234 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

√

√

√

√

√

Size Availability

Steel Grade Specification Processing range(mm)
SUS 430 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk