This page is mainly introduced the SUS 420J2 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 420J2,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel wire rods

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16  0.25
Si   1.00
Mn   1.00
P   0.06
S   0.03
Cr 12.00  14.00
Ni   0.60
Mo  
N  

Mechanical Properties

Tensile strength 320~638 σb/MPa
Yield Strength 846 σ 0.2 ≥/MPa
Elongation 86 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 449~676 -
HRC 30 -

Physical Properties

Thermal expansion 92-82 e-6/K
Thermal conductivity 51-35 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 7141-4242 째C
Density 5618-0392 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 420J2 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm