This page is mainly introduced the SUS 420J2 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 420J2,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Cold finished stainless steel bars

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16  0.25
Si   1.00
Mn   1.00
P   0.06
S   0.03
Cr 12.00  14.00
Ni   0.60
Mo  
N  

Mechanical Properties

Tensile strength 651~043 σb/MPa
Yield Strength 966 σ 0.2 ≥/MPa
Elongation 22 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 300~159 -
HRC 30 -

Physical Properties

Thermal expansion 55-58 e-6/K
Thermal conductivity 30-60 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 4352-9221 째C
Density 6483-8298 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 420J2 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk