This page is mainly introduced the CNS 631 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of CNS 631,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel bars

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.09
Si   1.00
Mn   1.00
P   0.040
S   0.030
Ni 6.50  7.75
Cr 16.00  18.00
Cu  
Al 0.75  1.50

Mechanical Properties

Tensile strength 321~234 σb/MPa
Yield Strength 224 σ 0.2 ≥/MPa
Elongation 27 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 332~651 -
HRC 30 -

Physical Properties

Thermal expansion 69-91 e-6/K
Thermal conductivity 88-40 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 2812-3917 째C
Density 1956-4997 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
CNS 631 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk