This page is mainly introduced the CNS 630 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of CNS 630,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel bars

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.07
Si   1.00
Mn   1.00
P   0.040
S   0.030
Ni 3.00  5.00
Cr 15.50  17.50
Cu 3.00  5.00
Nb 0.15  0.45

Mechanical Properties

Tensile strength 408~196 σb/MPa
Yield Strength 596 σ 0.2 ≥/MPa
Elongation 28 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 375~338 -
HRC 30 -

Physical Properties

Thermal expansion 44-73 e-6/K
Thermal conductivity 84-76 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 3031-8567 째C
Density 2737-6565 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
CNS 630 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:630
Previous: 440F
Next: CNS 631